uncured 2 part epoxy

Submitted by Guy on 11/28/04 at 6:12 PM. ( GUYPETERS83@HOTMAIL.COM ) 24.118.103.191

Help. I just glossed several fish with a 2 part epoxy, Klear Koat, measured well and mixed well with a whip and a drill. now 2 of the fish wont cure to a tack free finish. Its been a week and they are still tacky. What can I do if anything to get this epoxy to hard cure? Please refrain from any sarcastic remarks.

Return to The Taxidermy Industry Category Menu


Warm them up?

This response submitted by Cecil on 11/28/04 at 7:27 PM. ( ) 64.184.33.225

Worth a try.


Guy

This response submitted by Jeff F. on 11/28/04 at 8:10 PM. ( NaturesTrophies,aol ) 152.163.100.135

In all seriousness. Why not call the manufacturer and get specific instructions? Seems pretty simple.(IMHO) Hope it works out. Jeff F.


Yes, heat them up.

This response submitted by Old Pro Taxidermist on 11/28/04 at 8:18 PM. ( ) 69.171.249.149

Cecil is correct. Place the fish in a small, HEATED area 100 degrees for 24 hours. If that does not work, the epoxy is defective.